Default Agitation

Starting to get info together on building a 45 gallon line. Currently I am not using any agitation except in the ano bath. I have read where some guys are using agitation in all their tanks? I understand why but just wondering how many of you are doing this?
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #2 (permalink)  
Old 11-15-2006, 07:41 PM
acidrain's Avatar
Metal Finishing Guru
 
Join Date: Sep 2004
Posts: 1,181
acidrain has a spectacular aura aboutacidrain has a spectacular aura about
Default Re: Agitation

Not me, but I am considering it for the strip/etch and the dye tanks.
__________________
I do things.
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #3 (permalink)  
Old 11-15-2006, 09:02 PM
Amateur Metal Finisher
 
Join Date: Feb 2006
Posts: 109
hurricaneracing is on a distinguished road
Default Re: Agitation

Me too. I plan to start building at the first of the year. Just want to do it once.
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #4 (permalink)  
Old 11-15-2006, 11:40 PM
destroyer125's Avatar
Experienced Metal Finisher
 
Join Date: Jul 2005
Posts: 447
destroyer125 is an unknown quantity at this point
Default Re: Agitation

I just use it in the anodizing tank....Hand swirling the part around in the dye is good enough agitation for me
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
Closed Thread

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


Similar Threads
Thread Thread Starter Forum Replies Last Post
Agitation purpose??? hurricaneracing Anodizing Questions 27 09-13-2006 11:06 AM
Agitation ??? hurricaneracing Anodizing Questions 1 08-30-2006 04:53 AM
possible agitation idea??? bigbear Anodizing Questions 5 07-30-2006 02:25 AM
Air agitation or pump? rick201 Anodizing Questions 2 04-19-2006 02:04 AM
My agitation solution NeoMoses Anodizing Questions 35 10-20-2004 04:55 PM


All times are GMT -4. The time now is 08:01 AM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2009, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.3.0
Copyright © Caswell Inc.