  #21 (permalink)  
Old 03-02-2007, 10:58 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,374
Blog Entries: 2
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default Re: what went wrong?

The secret of this system is that WE have a plan! The LCD plan!

If you follow it to the letter, and defend it rigorously whenever a newbie comes along with his version, you will always prevail. He will be converted to LCD, and it will save us all a lot of typing.


Thanks guys, for sticking o the plan.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #22 (permalink)  
Old 03-18-2007, 07:05 AM
Newbie
 
Join Date: Dec 2006
Posts: 31
dewil is on a distinguished road
Default Re: what went wrong?

My latest piece. Orange 3a with deep red in it. About 15cc red/ ½gallon orange. Matches the KTM very well.

Its done with 6 ASF for 2h. The CC powersource makes it all soo much easier and I also bought an aquarium-pump to swirl the water and make a more even temp and it works wonders. Huge difference in anodize thickness, much more even.
Here is a couple of pics.
what went wrong?-dsc00203mindre.jpg

what went wrong?-daemparn.jpg
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #23 (permalink)  
Old 03-19-2007, 02:17 AM
Newbie
 
Join Date: Feb 2007
Posts: 12
Hard_Color is on a distinguished road
Default Re: what went wrong?

Quote:
Originally Posted by dewil
My latest piece. Orange 3a with deep red in it. About 15cc red/ ½gallon orange. Matches the KTM very well.

Its done with 6 ASF for 2h. The CC powersource makes it all soo much easier and I also bought an aquarium-pump to swirl the water and make a more even temp and it works wonders. Huge difference in anodize thickness, much more even.
Here is a couple of pics.
Attachment 687

Attachment 688

WOW that is very very nice! That color is awesome, thanks for sharing it!
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
Closed Thread

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


Similar Threads
Thread Thread Starter Forum Replies Last Post
Help, I'm doing spmething wrong autoshopowner Powder Coating Questions 3 11-08-2006 08:13 PM
Can you figure out what I did wrong? cruizer Powder Coating Questions 11 07-17-2006 04:34 PM
Cartridge rolls - description wrong? mpierich Caswell Please Sell This... 1 06-15-2005 12:52 AM
Ok,what am I doing wrong mach1man Metal Polishing Questions 1 08-18-2004 08:31 PM
What's wrong here...... dsacco1013 Powder Coating Questions 2 01-05-2004 11:15 PM


All times are GMT -4. The time now is 04:38 PM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2009, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.3.0
Copyright © Caswell Inc.