Question Masking or Carving

Hello guyz, i'm a noobie in this forum. How can i achieve to make the logo in this picture?
Is it through masking or carving with laser? TQ 4 the inputs....

Last edited by oddyseus; 03-01-2007 at 11:12 PM.
Reply With Quote
  #2 (permalink)  
Old 03-01-2007, 11:23 PM
Newbie
 
Join Date: Feb 2007
Location: Kansas City, MO
Posts: 50
kco1196 is on a distinguished road
Send a message via Yahoo to kco1196
Default Re: Masking or Carving

I've read you can do things like that by masking. Making a fine line might be a challenge.
Reply With Quote
  #3 (permalink)  
Old 03-01-2007, 11:51 PM
Newbie
 
Join Date: Feb 2007
Posts: 4
oddyseus is on a distinguished road
Default Re: Masking or Carving

Thx for the input bro....really appreciate it
Reply With Quote
  #4 (permalink)  
Old 03-02-2007, 08:56 AM
Amateur Metal Finisher
 
Join Date: Sep 2002
Posts: 96
Tim Wiltse
Default Re: Masking or Carving

That is engraved for sure. Look above the "c" in "racing". The cutter bounced a little ...see the little dots instead of a solid line. Something that small can't be masked. They didn't have the part centered in the machine I might add! See how the end runs off the side of the parts. Looks like a neck clamp or seat post clamp?

Later,
Tim
Reply With Quote
  #5 (permalink)  
Old 03-04-2007, 01:01 AM
Metal Finishing Guru
 
Join Date: Sep 2004
Posts: 781
acidrain is on a distinguished road
Default Re: Masking or Carving

Laser engraving is an excelent way to reproduce those effects.
__________________
Specializing in anodized graphics in Paintball guns.
Reply With Quote
  #6 (permalink)  
Old 03-04-2007, 10:23 AM
Amateur Metal Finisher
 
Join Date: Sep 2002
Posts: 96
Tim Wiltse
Default Re: Masking or Carving

It sure would! And laser engraving would give a better finish too.

LAter,
Tim
Reply With Quote
  #7 (permalink)  
Old 03-04-2007, 10:17 PM
Newbie
 
Join Date: Feb 2007
Posts: 4
oddyseus is on a distinguished road
Post Re: Masking or Carving

Does anyone got a link where i can get those laser engraving machine?, i'm located in Indonesia. Besides laser, can i use other engraving machine which is more economical in cost? Has anyone use this kinda laser machine? Thx b4
Reply With Quote
  #8 (permalink)  
Old 03-05-2007, 07:13 PM
Amateur Metal Finisher
 
Join Date: Sep 2002
Posts: 96
Tim Wiltse
Default Re: Masking or Carving

I don't have a link right off hand but a low end small laser engraving machine will run you arond $2,000 give or take and goes up from there.

LAter,
Tim
Reply With Quote
  #9 (permalink)  
Old 03-05-2007, 11:12 PM
destroyer125's Avatar
Experienced Metal Finisher
 
Join Date: Jul 2005
Posts: 437
destroyer125 is an unknown quantity at this point
Default Re: Masking or Carving

epilog.com makes some very nice lasers, however, their smallest laser starts at $10,000
Reply With Quote
  #10 (permalink)  
Old 03-06-2007, 02:39 AM
Newbie
 
Join Date: Feb 2007
Posts: 4
oddyseus is on a distinguished road
Default Re: Masking or Carving

Quote:
Originally Posted by Tim Wiltse
I don't have a link right off hand but a low end small laser engraving machine will run you arond $2,000 give or take and goes up from there.

LAter,
Tim
I got this link from googling www.able-engravers.com . And i've contacted them via e-mail, but poorly they don't ship outside North America
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Masking products? SX Paintball Anodizing Questions 4 02-14-2007 12:59 AM
Is thin sheet acrylic ok for masking? ld2222 Electroplating Questions 1 12-15-2004 10:29 PM
Looking for a MASKING product for blasting ops Halliwell1 Other Metal Finishing Questions 3 04-21-2004 07:23 PM
Masking products for EN plating? edclark Electroplating Questions 0 12-23-2003 03:41 PM
Looking for masking tape recomendations. chcarver Metal Polishing Questions 0 03-06-2003 02:51 PM


All times are GMT -4. The time now is 03:26 PM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.