Hello, just wondering if anyone air agitates there dyes. I never have done this, however this past weekend I did some sample pieces and with new caswells gray dye had little dark spots on my part, also did some pink parts and turned out awesome. Just wondering if the dye needed to be agitated?
Thanks, Shane |
|
|||
|
Agitation is certainly an option... been considering it myself.
I suggest AT LEAST giving the dye a stir before dunking the parts. Also, the dye will thoroughly mix in after it is brought to temperature. Be careful not to let the parts rest against the walls of the tank or touch each other or there may be dark areas.
__________________
Specializing in anodized graphics in Paintball guns. |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| possible agitation idea??? | bigbear | Anodizing Questions | 5 | 07-30-2006 01:25 AM |
| Air agitation or pump? | rick201 | Anodizing Questions | 2 | 04-19-2006 01:04 AM |
| Sandblasting and prepping, newb help me! | emopunk96 | Powder Coating Questions | 15 | 04-18-2006 12:53 PM |
| powder dyes vs concentrate liquid dyes | whistule | Anodizing Questions | 3 | 08-21-2003 10:06 PM |
| Lead plates, anodising voltages and dyes | whistule | Anodizing Questions | 2 | 08-17-2003 09:58 PM |