Is it safe to anodize say 60xx & 70xx parts at the same time? Or should they be divided into two separate jobs?
Reply With Quote
  #2 (permalink)  
Old 04-20-2007, 02:33 PM
destroyer125's Avatar
Experienced Metal Finisher
 
Join Date: Jul 2005
Posts: 428
destroyer125 is an unknown quantity at this point
Default Re: Mixing allows

The only thing suggested to be isolated from other alloys is 2xxx series
Reply With Quote
  #3 (permalink)  
Old 04-20-2007, 03:10 PM
Newbie
 
Join Date: Feb 2007
Location: Kansas City, MO
Posts: 48
kco1196 is on a distinguished road
Send a message via Yahoo to kco1196
Default Re: Mixing allows

So I would just add up the surface area of all parts both 60xx & 70xx, determine my thickness and ASF then go from there? That sounds way to easy.
Reply With Quote
  #4 (permalink)  
Old 04-20-2007, 05:50 PM
destroyer125's Avatar
Experienced Metal Finisher
 
Join Date: Jul 2005
Posts: 428
destroyer125 is an unknown quantity at this point
Default Re: Mixing allows

at 12v current density, 7xxx needs to be anodized 3/4 the time you would for 6061...at 15v it need to be anodized for 1/2 the time to get right at a 1 mil coating.
Reply With Quote
  #5 (permalink)  
Old 04-20-2007, 07:47 PM
Newbie
 
Join Date: Feb 2007
Location: Kansas City, MO
Posts: 48
kco1196 is on a distinguished road
Send a message via Yahoo to kco1196
Default Re: Mixing allows

I'm not sure I understand what you are trying to tell me Destroyer. Are you saying that I will need to pull the 70xx parts out sooner?
Reply With Quote
  #6 (permalink)  
Old 04-21-2007, 02:25 PM
destroyer125's Avatar
Experienced Metal Finisher
 
Join Date: Jul 2005
Posts: 428
destroyer125 is an unknown quantity at this point
Default Re: Mixing allows

Yes I am, it will anodize faster then plain 6061
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
color mixing pokchop Oven Building Forum 9 04-22-2006 11:50 AM
Mixing the pickle Baths Tim1hd Electroplating Questions 4 05-10-2005 05:02 PM
MIXING POWDERS turch Powder Coating Questions 7 12-01-2004 10:00 PM
Dye mixing and fluorescent colors sgunn911 Anodizing Questions 17 10-18-2004 01:11 PM
Mixing Black Oxide CarveJunky Other Metal Finishing Questions 0 08-19-2003 08:23 AM


All times are GMT -4. The time now is 04:31 AM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.