Hi Guys!!!

Another Prob......
I tried to mix some olive dye to reach the color of the ego-pic at the end of the post.....
My add. problem here in Germany.....I don't have the Caswell products.

Would be great, if anybody could tell me how to mix a nice olive with basic color dyes, 'cause I've no empty bottles left to store all the shades of green from my tries Forrest Green, Wimbledon Green, Poison Green.......no problem, only ***** olive doesn't work properly....

There was something.........mixing little amounts of black into yellow......but I don't remember......

I need your help, PLEASE.....
Greetinx Alex

mixing-olive-dye-egonimme.jpg

Last edited by LOON; 06-01-2007 at 11:57 AM.
Reply With Quote
  #2 (permalink)  
Old 06-01-2007, 09:40 PM
Metal Finishing Guru
 
Join Date: Sep 2004
Posts: 785
acidrain is on a distinguished road
Default Re: Mixing Olive Dye

Mostly orange, mixed with black and green (maybe some red) makes a nice OD.
__________________
Specializing in anodized graphics in Paintball guns.
Reply With Quote
  #3 (permalink)  
Old 06-02-2007, 12:15 AM
destroyer125's Avatar
Experienced Metal Finisher
 
Join Date: Jul 2005
Posts: 439
destroyer125 is an unknown quantity at this point
Default Re: Mixing Olive Dye

I like caswells stock color, it isnt like the paintball OG's tho. The paintball OG's are more of a baby poop color.
Reply With Quote
  #4 (permalink)  
Old 06-02-2007, 03:04 AM
Newbie
 
Join Date: Apr 2007
Posts: 39
LOON is on a distinguished road
Default Re: Mixing Olive Dye

You guys are great.....that's what I needed
I'll try it, ....hopefully not the baby-poo-version

THANK YOU!!!

Alex Rueland
Reply With Quote
  #5 (permalink)  
Old 06-02-2007, 12:58 PM
Newbie
 
Join Date: Apr 2007
Posts: 39
LOON is on a distinguished road
Default Re: Mixing Olive Dye

mixing-olive-dye-loonytunez-oliv-002.jpg

That's the result......
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
mixing gold with yellow to get more a gold blackcote Anodizing Questions 6 05-27-2007 10:35 PM
Where can I find Flat Olive Drab powder? kcenicola Powder Coating Questions 1 04-16-2007 06:10 PM
Black dye gbtweedy Anodizing Questions 2 12-29-2006 07:00 PM
Black anodize dye doesn't take AlanJB Anodizing Questions 1 09-18-2006 10:19 PM
7000 series parts dye, but 6000 series won't acidrain Anodizing Questions 20 11-17-2005 10:19 PM


All times are GMT -4. The time now is 03:01 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.