Default newest piece would love some suggestions

constructive criticism welcomed.

any suggestions i already bleached it back out i had a nasty finger print on one side did it all by hand ano'd at 4.25A for 90 mins for just the feedneck and body the reg adapter was already done would love some fade suggestions.
Reply With Quote
  #2 (permalink)  
Old 06-28-2007, 03:15 AM
Experienced Metal Finisher
 
Join Date: Jan 2003
Posts: 321
chromo
Default Re: newest piece would love some suggestions

Well I don't have that good of view in that picture.
A few suggestions though.

Make sure your have the right gloves, I think Nitrial? Keep all oils and finger prints off the work. Not sure what you want to do there. FADE? Dye one side maybe, flip over and dye other side. Flow? Sink into dye to most wanted fad area, slowly remove from dye. Top most part dyed the weakest as removed first. Lower parts dyed the most as left in longer.
Send better photos of the work, less of the body LOL

Stop working in the nude!
OR if female, Send better pictures. LOL
Reply With Quote
  #3 (permalink)  
Old 06-28-2007, 03:53 PM
Newbie
 
Join Date: Jun 2006
Location: Riga, MI
Posts: 39
PBInferno is on a distinguished road
Send a message via AIM to PBInferno
Default Re: newest piece would love some suggestions

Looks pretty good, but I'd make so there's more of a fade. It's a little too abrupt of a transition in that picture.
EDIT: Why are you not wearing any clothes?
__________________
•Inferno Custom Paintball•
Reply With Quote
  #4 (permalink)  
Old 06-28-2007, 09:04 PM
Metal Finishing Guru
 
Join Date: Sep 2004
Posts: 887
acidrain is on a distinguished road
Default Re: newest piece would love some suggestions

Wider fade area...
I think chromo was speaking to it as well. Spend less time at the end of your dip. What I do is fully dip and hold for awhile at the begining of the fade area, slowly dip further, then speed up the dip at the end. Then, really quickly, pull out and dip in clean rinse. That way, the very end of the dye area only spends a split second in the dye.
Also, you picked colors that dye really quickly, so they are hard to control without leaving a hard line. Try lower the dye temp, and you'll see that the dye takes longer, and therefor more controllable.
__________________
Specializing in anodized graphics in Paintball guns.
Reply With Quote
  #5 (permalink)  
Old 06-28-2007, 09:16 PM
Newbie
 
Join Date: May 2007
Posts: 32
starns is on a distinguished road
Default Re: newest piece would love some suggestions

lol i had my shirt off guys and the dyes where both at Room temp teal seems to want to take all or none..
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
well got one piece done what do you guys think ekernel Metal Polishing Questions 3 12-12-2006 08:50 PM
LCD anodize of a large piece? scocklin Anodizing Questions 2 12-29-2004 01:21 AM
electroless chrome - larger piece? tww Electroplating Questions 3 03-18-2003 08:18 PM


All times are GMT -4. The time now is 01:41 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.