Default Success on first try

This weekend I spent time anodizing for the first time.
Read the book, read the posts, got the DVD mixed the chems, struggled somewhat with keeping good connections to the parts and found out how to re-establish anode-part connections, built a small collection of aluminum wire connectors and hardly screwed up anything after running the test pieces.
This was my first real attempt at anodizing and the Caswell system works pretty darn good.
I'll try to post a pic of the parts. Black is what I needed this time, later I'll try red.
Reply With Quote
  #2 (permalink)  
Old 10-22-2007, 05:33 PM
Metal Finishing Guru
 
Join Date: Sep 2004
Posts: 889
acidrain is on a distinguished road
Default Re: Success on first try

Wow, really good work... it's amazing when a plan comes together, isn't it?!
__________________
Specializing in anodized graphics in Paintball guns.
Reply With Quote
  #3 (permalink)  
Old 10-22-2007, 11:20 PM
Newbie
 
Join Date: Nov 2004
Posts: 17
andyrayk
Default Re: Success on first try

Having trouble uploading pics. I've set up an album but can't put anything into it or post an attachment to my posts. Never had a problem with ANY other sites. Must be missing something simple too. I pick the pic to upload and hit submit be keep getting an error message that says "Unable to move/copy file " . It can't be this hard. Tried from two different computers.
The file is only a 86kb jpg.

Last edited by andyrayk; 10-22-2007 at 11:25 PM.
Reply With Quote
  #4 (permalink)  
Old 10-29-2007, 08:40 AM
Amateur Metal Finisher
 
Join Date: Jun 2004
Posts: 99
blackcote
Send a message via AIM to blackcote Send a message via MSN to blackcote
Default Re: Success on first try

I too have been unable to upload anything in quite some time. might be worth asking caswell about.
__________________
Justin Martin, VP
Blackcote
RR1 Box 116
Liverpool, PA 17045
www.blackcote.com
blackcote@pa.net
Reply With Quote
  #5 (permalink)  
Old 11-01-2007, 08:19 PM
Newbie
 
Join Date: Nov 2004
Posts: 17
andyrayk
Default Re: Success on first try

Dunno what can be done.
Must be a secret handshake so something.
I've tried too many times.
I will no longer waste any more time and effort
on this problem.
I've got lotsa stuff to coat.
Reply With Quote
  #6 (permalink)  
Old 11-02-2007, 12:42 AM
Amateur Metal Finisher
 
Join Date: Sep 2005
Posts: 65
hvacman250 is on a distinguished road
Default Re: Success on first try

Use Putfile. Very easy. See:

Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Copy Cad - Success with first time plating charlton Electroplating Questions 3 07-31-2005 02:04 PM
Success!!! squaredealer Metal Polishing Questions 0 09-24-2004 09:35 AM


All times are GMT -4. The time now is 04:40 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.