Old 12-03-2007, 12:44 PM
Amateur Metal Finisher
 
Join Date: Jul 2007
Posts: 98
Empire03 is on a distinguished road
Default Re: Need a list please.

Alright, but that still doesn't solve the bath heating....
Reply With Quote
  #12 (permalink)  
Old 12-03-2007, 07:51 PM
sswee's Avatar
Moderator
 
Join Date: Nov 2004
Location: close to Austin, Texas
Posts: 1,212
sswee is a jewel in the roughsswee is a jewel in the roughsswee is a jewel in the roughsswee is a jewel in the rough
Default Re: Need a list please.

Which bath?
If you're referring to the anodize tank, a glass tube aquarium heater will work.
SS
Reply With Quote
  #13 (permalink)  
Old 12-03-2007, 08:27 PM
Amateur Metal Finisher
 
Join Date: Jul 2007
Posts: 98
Empire03 is on a distinguished road
Default Re: Need a list please.

alright thx for that i ust bought a 500 watt glass heater with digital thermometer hope it works
Reply With Quote
  #14 (permalink)  
Old 12-04-2007, 05:50 PM
Amateur Metal Finisher
 
Join Date: Jul 2007
Posts: 98
Empire03 is on a distinguished road
Default Re: Need a list please.

umm im kinda confused here what is the name for the tan compound?
Reply With Quote
  #15 (permalink)  
Old 12-04-2007, 07:56 PM
Metal Finishing Guru
 
Join Date: Sep 2004
Posts: 833
acidrain is on a distinguished road
Default Re: Need a list please.

I use BLKBC5 (black) for cut, and BRBC5 (brown) for color... not quite sure why I picked that one, but seams to color out well, but does leave a good amount of residue that needs to be cleaned off.
Maybe this one would work well too (or even better): F515-6126.
What are the rest of you guys using?
__________________
Specializing in anodized graphics in Paintball guns.
Reply With Quote
  #16 (permalink)  
Old 12-04-2007, 08:14 PM
Amateur Metal Finisher
 
Join Date: Jul 2007
Posts: 98
Empire03 is on a distinguished road
Default Re: Need a list please.

ok thx for the clarification now can i get some help with the temps.


for the annodizing bath should be at or close to 70* correct?
the dye should be at 140* correct?
the sealer should be at 180* correct?

does the desmut and stripper have to be heated?
Reply With Quote
  #17 (permalink)  
Old 12-04-2007, 09:04 PM
Metal Finishing Guru
 
Join Date: Sep 2004
Posts: 833
acidrain is on a distinguished road
Default Re: Need a list please.

Correct...
I heat both the De-smut and degreaser to 140F as well, but I'm not sure that's what is recommended... it will say on the package.
__________________
Specializing in anodized graphics in Paintball guns.
Reply With Quote
  #18 (permalink)  
Old 12-04-2007, 09:25 PM
Amateur Metal Finisher
 
Join Date: Jul 2007
Posts: 98
Empire03 is on a distinguished road
Default Re: Need a list please.

alright thx once again one more question tho. lol the dye gold s is that used for gold of is yellow?
Reply With Quote
  #19 (permalink)  
Old 12-04-2007, 11:53 PM
Metal Finishing Guru
 
Join Date: Sep 2004
Posts: 833
acidrain is on a distinguished road
Default Re: Need a list please.

The Gold S is a very nice gold.
Polish to a brilliant shine, then ano to only .5mil. Then dye for a relatively short period of time (2 to 5 minutes?). To me, a lighter color looks more like real gold.
__________________
Specializing in anodized graphics in Paintball guns.
Reply With Quote
  #20 (permalink)  
Old 12-05-2007, 10:42 PM
Amateur Metal Finisher
 
Join Date: Jul 2007
Posts: 98
Empire03 is on a distinguished road
Default Re: Need a list please.

Ok, I have a few more questions for you guys.

1.What's the advantage to having a bigger annodizing bath?Besides fitting more parts.

2.How do I strip the anno inside of breeches?Does the stripper do it on its own?

3.How exactly do I measure the area of parts?I know how to find basic area,like rectangles,triangles,and circles.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Alloy list? jc88usus Anodizing Questions 6 08-16-2007 01:23 PM
My Buildup List JNizzle Oven Building Forum 3 06-12-2007 10:43 PM
The Final List of Materials! TreyY Oven Building Forum 19 05-29-2006 07:53 PM
Starter List grommit Powder Coating Questions 0 03-30-2006 03:22 AM
Shopping List buzzurd Metal Polishing Questions 0 01-10-2004 05:32 PM


All times are GMT -4. The time now is 10:02 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.