Default Anodizing

I'm in the process of anodizing. I dont know much. I'm wondering where i can get a digital constant current 25A-50A power supply. Thanks
Reply With Quote
  #2 (permalink)  
Old 01-09-2008, 06:44 AM
Newbie
 
Join Date: Jun 2007
Posts: 22
LIVVI is on a distinguished road
Default Re: Anodizing

Hello

Here is a start. MASTECH VARIABLE REGULATED DC P. S(HY3030E) 0-30V/0-30A. This one is on ebay there are more of course. I bought a HY2030 from a power seller on ebay.
Reply With Quote
  #3 (permalink)  
Old 01-09-2008, 09:20 AM
Amateur Metal Finisher
 
Join Date: May 2006
Posts: 73
mkriegs is on a distinguished road
Default Re: Anodizing

I bought a mastech as well and haven't had any problems with it
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Part not anodizing/Partially anodizing taylorm Anodizing Questions 4 07-16-2004 04:57 PM


All times are GMT -4. The time now is 01:26 AM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.