Default black dye

im having trouble with my black dye, there is no way i can achieve the desired color, all my tries ended up looking dark blue!!?, what is goin on.
Reply With Quote
  #2 (permalink)  
Old 01-19-2008, 01:28 PM
Metal Finishing Guru
 
Join Date: Sep 2004
Posts: 750
acidrain is on a distinguished road
Default Re: black dye

Either the dye is not hot enough, or you didn't ano long enough. Black needs 1mil for a nice deep black.
If this is 6xxx series, and all your previous attempts were with 7xxx, there will be a difference. 7xxx will ano faster than 6xxx. Try about 25% more time if that's the case.
__________________
Specializing in anodized graphics in Paintball guns.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Black turns bronzy black blurrycustoms Anodizing Questions 11 12-25-2007 09:57 PM
Black Magic or Super wet Black? Which is best? chromo Powder Coating Questions 2 09-17-2007 06:55 PM
Super mirror black or low gloss black? Deecoat Powder Coating Questions 2 03-09-2006 10:24 PM
After 1500g sanding, and black emery, frame has black streak fizlfry Metal Polishing Questions 8 04-26-2005 10:09 AM


All times are GMT -4. The time now is 04:19 PM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.