Sure, the acidity eventually gets weakened and needs to be replaced.
Make sure to dispose of it properly at your municipal HAZMAT disposal center. Some service stations will also take battery acid for a price.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
|
||||
|
Probably not, but dump it properly anyway.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Anodizing Sealant LT | jqmah | Anodizing Questions | 0 | 06-17-2005 10:54 AM |
| maintaining wire flexibility after anodizing | aanan | Anodizing Questions | 1 | 02-13-2005 06:46 PM |
| "Hard" Anodizing vs. "normal"; differenc | dagobert | Anodizing Questions | 6 | 02-26-2004 11:24 PM |
| Color depth vs. anodizing time | NeoMoses | Anodizing Questions | 17 | 02-03-2004 09:06 PM |
| Anodizing different alloys | TONYZ | Anodizing Questions | 2 | 11-02-2003 01:31 PM |