i recently got the gold dye and have tried anodizing a few pieces with it, the problem i have is that i've only gotten 2 pieces to actually look gold in color. i did 5 pieces at the same time and all the other ones came out more of an orange color than gold. i even reanodized the other pieces and left them in the dye for less time and the same thing happens.
|
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Question on gold plating | oldtoys1961 | Electroplating Questions | 4 | 05-07-2008 10:41 PM |
| Question about gold plating a gun | arny068 | Electroplating Questions | 1 | 03-26-2005 12:18 PM |
| How about Gold on Gold ? | Ra | Electroplating Questions | 5 | 10-12-2004 07:47 PM |
| Question on gold plating brass. | oldtoys1961 | Electroplating Questions | 2 | 12-29-2003 04:45 PM |
| Gold Plating Question | Rusty Armstrong | Electroplating Questions | 2 | 03-21-2002 07:12 PM |