i just tried the lt sealant and did it by the directions and it stripped all the dye off my piece, it was only in there a few minutes. after spending hours getting my pieces ready and anodized then this happens kinda made me pretty mad
Reply With Quote
  #2 (permalink)  
Old 06-29-2003, 06:39 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,367
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

Hmmm, it doesn't do this by design. It's a sealant not a stripper and is a commercial grade sealing product (used by large anodizing shops all over the world)

If you can provide some more details to us, using our support section, we'll help you figure out exactly what went wrong.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
  #3 (permalink)  
Old 07-14-2003, 09:55 PM
Newbie
 
Join Date: May 2003
Location: nh
Posts: 29
dropride
Default

whenever i use the lt sealant it turns the part hazy when it dries, the only way ive found to take it off is to use mothers polish, is this supposed to happen?
Reply With Quote
  #4 (permalink)  
Old 07-16-2003, 04:35 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,367
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

Can you please send us a picture of this? We've not heard of this happening before. PLease send to support@caswellplating.com

Thanks
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Anodizing Sealant LT jqmah Anodizing Questions 0 06-17-2005 10:54 AM
Splotchy anodize or dye result sccc Anodizing Questions 19 09-01-2004 12:51 PM
annodizing sealant safe for parts... djxmetal Anodizing Questions 3 11-06-2003 10:28 PM
LT sealant questions desert_roamer Anodizing Questions 1 07-09-2003 06:01 PM
Low temp. anodize sealant tool_man Anodizing Questions 2 03-12-2003 08:07 PM


All times are GMT -4. The time now is 02:04 AM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.