Default Metal Not taking color....

I have a bar of aluminum that im practicing on and I leave it in teh anodize for 30min @55-65 amps and 12volts and then i put in 140degree red dye for 25min and i took it out and no color,

And how do you do fades (Eg yellow to black?)
Reply With Quote
  #2 (permalink)  
Old 07-11-2003, 10:52 AM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,366
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

Most places do these sort of effects by anodizing in one color first, then masking off certain areas you want a pattern to appear on (our Maskit product works well for this), then stripping the anodize.

The area that was masked won't strip and the color will remain. Then re-anodize the part a different color and repeat until you get the desired result.

I know you've posted your problem on PRS, with more details about your application, so it will be answered there. The first thing you should check is "does the part have an anodize layer?" You check this with a multimeter. If the part is not conductive, it has been anodized. We'll wait for your answer on PRS.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
PLATING POT METAL............... 48Buick Plating Pot Metal 31 08-29-2007 11:40 AM
Plating over cold metal casting jh2ohouse Electroplating Questions 2 12-16-2006 08:28 PM
Color depth vs. anodizing time NeoMoses Anodizing Questions 17 02-03-2004 09:06 PM
Refinishing Metal Golf Club Heads BillSchultz Other Metal Finishing Questions 0 08-17-2003 10:40 AM
color fade anno krazi_ivan Anodizing Questions 0 04-13-2003 11:40 PM


All times are GMT -4. The time now is 02:54 AM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.