Smile copy chrome luck

First off I want to tell everyone Marry Christmas. I got a 4.5gal copy chrome kit almost two years ago and through trial and error have gotten quite good at plating. Good enough in fact that I have the only shop in my county where the public can get parts plated. A word of advise for all the newbies is to just do as the manual tells you and be very meticulas in your preperation. I am currently enlarging my system and am having very good luck with the copy chrome system for all my plating needs. I have not gotten a defective piece back since I began this little venture a year ago. Thanks Caswell and the support staff.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
triple chrome vs. nickel/chrome vs. copy chrome spectraflamed Electroplating Questions 4 01-21-2007 10:07 AM
copy chrome vs triple chrome plating splbnd27 Electroplating Questions 18 06-21-2006 07:35 AM
so long and good luck to every one !!!!!!! customandsound Metal Polishing Questions 2 12-21-2004 12:07 AM
Had good luck with chrome powder! Hemi-T Powder Coating Questions 4 07-12-2003 02:21 AM
tripple chrome, nickel chrome, copy chrome or electroless ch magfinpete Electroplating Questions 1 05-19-2002 12:52 PM


All times are GMT -4. The time now is 10:18 AM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.