Let me start with saying thanks for all of the valuable info on this forum. It has helped me a great deal. My ?? is can I replate copy chrome over copy chrome or does it need to be stripped? I have some small parts that I buffed a bit to much from and need to replate. I get the dull grey coat as well and plan on trying the technique mentioned here.
|
|
||||
|
If there are no defects in the plating that you are referring to then you can use the pickle #3 (one part of water, two parts battery acid allow to cool the add one more part of battery acid) immerse for 15-30 seconds, rinse then plate with the copy chrome.
__________________
-- Craige Brooks Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| copy chrome vs triple chrome plating | splbnd27 | Electroplating Questions | 18 | 06-21-2006 07:35 AM |
| Differet copper plating questions, plus copy chrome/ nickel? | krsimulis | Electroplating Questions | 1 | 07-26-2004 12:25 AM |
| Electroless Krome VS Copy Chrome plating? | qwik3r | Electroplating Questions | 3 | 04-28-2004 11:39 PM |
| Copy Chrome Start-up | Elitefisherman | Electroplating Questions | 10 | 04-18-2004 04:24 AM |
| Price of Copy Chrome vs. electroless Krome plating | dwthomas | Electroplating Questions | 1 | 05-14-2003 10:01 AM |