Either kit will provide a lasting finish if the items are processed correctly. The advantage to copy chrome is that it requires less amperage per square inch than chrome. The chrome kit will give you the chemicals necessary to plate onto plastics except for the conductive paint. Once the part is painted it needs to be immersed in the acid copper for at least 15 minutes before plating with either nickel (then chrome) or copy chrome.
__________________
-- Craige Brooks Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
|
|||
|
Craig, Thanks for the post. How do you know what size kit to buy. Is there any good advise for building tanks? I want to plate some long skinny parts.
Why only 15 minutes in the copper. I thought you needed to plate heavy enough with copper to metal finish the copper before plating with nickle or chrome? |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| How much clearance is needed? | JeffL | Oven Building Forum | 7 | 03-12-2006 09:45 AM |
| Seeking advise on PC and polishing as a living | LeeParsons | Powder Coating Questions | 7 | 08-01-2005 12:45 AM |
| Input needed by some of the inhouse pro's..... | Sid03 | Anodizing Questions | 20 | 01-15-2004 12:46 PM |
| Advise Needed! Hobby or Business? | mccain1976 | Electroplating Questions | 6 | 06-09-2003 10:50 PM |
| Nickel Replate: acid etch still needed after mechanical stri | xiphmont | Electroplating Questions | 4 | 05-13-2003 11:57 PM |