Imay of posted in the wrong place, please, forgive me, Seems with my Copy Cad system i am getting to much foam. its to the point where i cannot see my parts being plated. Foam is almost over flowing my plastic bucket, is there a anti foaming adgant i can use to correct this problem?? I don,t know what else to try?? open for suggestions! please help!!
|
![]() |