    I have been having problems getting a good plate on aluminum seems to get good in most areas but some rough areas also . My question is would flash copper before copy chrome elliminate that problem. I have tried every thing possible , My steel parts come out fine. I don't know were to go from here. Please help!!!! Thanks
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  2. Join Date
    Jul 2004
    Location
    Arkansas
    Posts
    295

    Re: Copy chrome ?

    yes you should be using copper befor you chrome aluminum
    Jim Eaton
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

+ Reply to Thread

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

     

Similar Threads

  1. triple chrome vs. nickel/chrome vs. copy chrome
    By spectraflamed in forum Electroplating Questions
    Replies: 4
    Last Post: 01-21-2007, 11:07 AM
  2. Copy chrome concern
    By jbvan in forum Electroplating Questions
    Replies: 2
    Last Post: 01-18-2007, 08:20 PM
  3. copy chrome vs triple chrome plating
    By splbnd27 in forum Electroplating Questions
    Replies: 18
    Last Post: 06-21-2006, 08:35 AM
  4. Copy Chrome Start-up
    By Elitefisherman in forum Electroplating Questions
    Replies: 10
    Last Post: 04-18-2004, 05:24 AM
  5. Copy Chrome Questions
    By junodale in forum Electroplating Questions
    Replies: 13
    Last Post: 03-17-2004, 12:15 PM

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts

Search Engine Friendly URLs by vBSEO 3.5.0 RC1 PL1