I'm wondering if anyone has had the idea of laying down a thick nickel plate (over copper if required) to give good corrosion protection then following up with a fairly thin cobalt plate to give the blue (as opposed to yellow) shine that will duplicate chrome? This would of course be very much the way real decorative chrome is used, over a thick nickel base plate which imparts the actual corrosion protection with the chrome only used to give a visual appeal (chrome being more blue than yellow tinted).
I would think this would give you a visually better part as compared to CopyKrome, which is a nickel/cobalt alloy. Using this two step process you would end up with all the cobalt on the surface layer which is where we really want it. |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Cobalt plating | mikekozura | Copy Chrome Kit Customers Only | 2 | 03-24-2008 03:51 PM |
| Still Looking for a cobalt blue | Livinincolor | Powder Coating Questions | 2 | 05-10-2007 10:54 PM |
| wanted: chrome/nickel plating for plastic trim (canada good but not necessary) | tinabanana | Services Offered/Wanted | 5 | 07-25-2006 01:24 PM |
| Nickel or chrome plating of fishing lures | yosemitegreg | Services Offered/Wanted | 3 | 07-16-2005 06:05 AM |
| Differet copper plating questions, plus copy chrome/ nickel? | krsimulis | Electroplating Questions | 1 | 07-26-2004 12:25 AM |