    Default Masking for brush plating

    I see Caswell has a product called Mask It. In a brush gold plating situation. Can this product be applied to a chrome piece, resist chrome stripping, resist nickel activation and still give a sharp edge to the gold plate up to the chrome?
    I've used the nail polish and acetone to remove routine but this is not acceptable due to other paint being in close proximity to the plated item.
    I'm looking for something I can apply with a brush or toothpick and peel off.
    Has anyone tried this product or have any ideas?
    Thanks,
    Eric

  2. #2
    Join Date
    Nov 2007
    Location
    Rochester NY
    Posts
    574

    Default Re: Masking for brush plating

    I've got some. It's fairly thick stuff. You can peel it right off, your best bet is to scribe it first and then peel it back, you'll get a really sharp line. I can send you a little bit of it if you want to try it out before you buy a 1/2 pint, I really don't use it all too often. Shoot me a pm.
    Quote Originally Posted by eric1001 View Post
    I see Caswell has a product called Mask It. In a brush gold plating situation. Can this product be applied to a chrome piece, resist chrome stripping, resist nickel activation and still give a sharp edge to the gold plate up to the chrome?
    I've used the nail polish and acetone to remove routine but this is not acceptable due to other paint being in close proximity to the plated item.
    I'm looking for something I can apply with a brush or toothpick and peel off.
    Has anyone tried this product or have any ideas?
    Thanks,
    Eric
    James Bateman

+ Reply to Thread

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

     

Similar Threads

  1. brush plating
    By azdave35 in forum Electroplating Questions
    Replies: 1
    Last Post: 09-19-2008, 01:02 AM
  2. 'Reverse' Brush Plating
    By Librum in forum Other Metal Finishing Questions
    Replies: 2
    Last Post: 09-09-2008, 04:20 AM
  3. Many questions about brush plating over old nickel plating
    By HowdeeDoodee in forum Electroplating Questions
    Replies: 5
    Last Post: 12-20-2007, 11:29 PM
  4. brush plating pot metal
    By goldmankc in forum Plating Pot Metal
    Replies: 3
    Last Post: 06-22-2007, 08:10 PM
  5. brush plating
    By rboyer in forum Electroplating Questions
    Replies: 1
    Last Post: 06-19-2007, 09:48 AM

Tags for this Thread

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts

Search Engine Friendly URLs by vBSEO 3.5.0 RC1 PL1