Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum  

Go Back   Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum > Electroplating Questions

Notices

Electroplating Questions Discussion Board For Electroplating and Electroless plating.

Reply
 
Thread Tools Display Modes
  #1 (permalink)  
Old 08-08-2003, 09:38 AM
Newbie
 
Join Date: Aug 2003
Posts: 6
c5mine
Default Plating automobile screws

I want to Chrome plug n plate small screws that attach the fascia to my Corvette. They are black screws and not sure what type of paint they used on it. I used DeKote to strip them but it did not work. What can I use to do this?
Reply With Quote
  #2 (permalink)  
Old 08-08-2003, 11:11 AM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,366
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

http://www.caswellplating.com/bbs/viewtopic.php?t=1117
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
  #3 (permalink)  
Old 08-08-2003, 12:26 PM
Newbie
 
Join Date: Aug 2003
Posts: 6
c5mine
Default

Thanks. I am now using the muratic acid. Looks like it is working. What next to prepare for plating?

Thanks!
Reply With Quote
  #4 (permalink)  
Old 08-08-2003, 06:17 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,366
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

Just rinse, degrease, rinse, and plate.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
  #5 (permalink)  
Old 08-09-2003, 12:04 PM
Newbie
 
Join Date: Aug 2003
Posts: 6
c5mine
Default

I plated all the screws and they all turned black. What am I doing wrong? Using the plug and plate copy chrome kit.
Reply With Quote
  #6 (permalink)  
Old 08-09-2003, 12:16 PM
Newbie
 
Join Date: Aug 2003
Posts: 6
c5mine
Default

OK. I have managed to get them silver with the copy chrome kit. How do i get them to shine. They are a silver color.
Reply With Quote
  #7 (permalink)  
Old 08-17-2003, 09:38 PM
Amateur Metal Finisher
 
Join Date: Jul 2002
Location: Florida
Posts: 69
gsw3 is on a distinguished road
Default

You have to polish the screws so they have a "chrome-like" finish prior to plating.
Your final plating will only look as good as the surface you are putting it on.
Of course you will also have to lightly polish the plated screws to bring up the shine.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Gold Plating and Nickel plating tzmandevil Electroplating Questions 2 09-16-2005 09:11 AM
Nickel bath inexplicably quits plating jackf Electroplating Questions 5 01-25-2005 09:55 PM
Plating screws? chromo Electroplating Questions 2 01-21-2003 03:17 PM
plating and size power? chromo Electroplating Questions 7 01-18-2003 02:52 AM
Electroless Krome plating Q's chcarver Electroplating Questions 1 10-10-2002 10:00 PM


All times are GMT -4. The time now is 06:43 PM.