Hi.
I need to know:
1. Muriatic acid mixing ratio for stripping zinc from steel parts.
2. Is alcohol (99% isopropyl or denaturated) a good degreaser for plating?
3. Your Plating Manual mentions using 1% sulf. acid to brighten zinc plate, will I be able to yellow chromate after that procedure or is this gonna be a clear chromated part already?
4. Compliment Jim McMillan and his wife on excellent service, I guess it is a company policy, but it just kicks butt!!! Deliveries the next day are a beautiful touch!
Thanks. Andrew.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
triple chrome vs. nickel/chrome vs. copy chrome spectraflamed Electroplating Questions 4 01-21-2007 11:07 AM
Copy Chrome? / Temp? hefrod Electroplating Questions 4 08-18-2005 03:47 PM
Copy Chrome Start-up Elitefisherman Electroplating Questions 10 04-18-2004 05:24 AM
Copy Chrome II on Pot Metal wbrown Plating Pot Metal 1 04-09-2003 09:15 AM
Copy chrome as a strike plate SUPRARACER Electroplating Questions 2 03-12-2003 03:36 PM


All times are GMT -4. The time now is 04:47 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.