lloyd
Default copychrome

I will be plating some nuts. Question is: the inside of the nuts will be in the shadow and I believe the threads will not plate. If this is correct then I don't have to figure the inside for surface area. Please let me know if I am right. Thank's in advance, Lloyd
Reply With Quote
  #2 (permalink)  
Old 08-26-2003, 11:28 AM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,357
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

They won't plate as heavily as the other areas, but they will plate and need to be part of your area calculations. To avoid this, you can mask off the inside threads, then you would NOT include them in the area.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
copychrome over silvaspray copierfixer Copy Chrome Kit Customers Only 5 04-11-2006 07:30 AM
Copychrome lloyd Electroplating Questions 2 10-06-2003 11:01 PM
Prep for copychrome lloyd Other Metal Finishing Questions 0 09-13-2003 08:24 PM
copychrome lloyd Other Metal Finishing Questions 2 08-03-2003 07:46 PM
Copychrome lloyd Electroplating Questions 2 07-27-2003 06:02 PM


All times are GMT -4. The time now is 10:07 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.