Default Well, I continue to fail...

...at getting any Copy Cad to work on any parts. I've been sandblasting them, putting them in the solution, turning on my rectifier, adjusting the amperage until it bubbles, etc. I pull the part out and it is silver. But the next morning, it's completely rusted--badly. My solution is now opaque and a kind of orange-brown, even after filtering it every time I try to use it. What the heck is going on?

I've already gone through the customer service process and nobody can figure out what is happening to make all my parts rust WHILE THEY ARE IN THE SOLUTION! I'm might order a 2-gallon setup so I can work in a larger container--the 1 gallon bucket is too small and I have a real hard time getting everything arranged for plating. This might be part of my problem?

Everyone else seems to have success with this--why don't I? Does anyone have any suggestions for what I could do to improve my odds before I drop another $100 on new solution and anodes? This is very frustrating...

Thanks in advance.
__________________
Matt Harwood
Harwood Performance Engineering
Cleveland, OH
Matt's 1941 Buick Century Restoration
Reply With Quote
  #2 (permalink)  
Old 09-09-2003, 10:39 PM
warchild's Avatar
Amateur Metal Finisher
 
Join Date: Feb 2003
Location: Seymour,Tn.
Posts: 147
warchild
Default

Could be something wrong with the wire you are useing to hang you stuff on maybe. i don't know if that would hurt anything but it mite be all it is.
__________________
WARCHILD
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


All times are GMT -4. The time now is 07:22 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.