Results 1 to 3 of 3

Thread: Plating Stainless Steel

  1. #1
    XK120DHC is offline Experienced Metal Finisher
    Join Date
    Jul 2004
    Location
    Texas! Is there anyplace else?
    Posts
    282

    Default Plating Stainless Steel

    Caswell's British Fasteners offers a couple of sizes of Spring Washers I am in need of, but they only have them in Stainless Steel.. The "factory correct" finish of these pieces on the car were originally Black Oxide. In the interested of Preservation, as well as restoration, I'm plating all the car's fasteners in "Black Zinc". That said, is there anything one can do to Stainless Steel (that won't ruin it) so it will accept the Zinc Plating and following Black Chromate??
    Charles

  2. #2
    seanc is offline Zinc Plating Guru
    Join Date
    Jun 2003
    Posts
    304

    Default Re: Plating Stainless Steel

    Charles:

    I'd say clean, prep & pickle as usual. I don't so SS parts, but it sticks just fine to SS danglers!

    Grab a couple of SS washers from a hardware store & try it.

    Sean

  3. #3
    XK120DHC is offline Experienced Metal Finisher
    Join Date
    Jul 2004
    Location
    Texas! Is there anyplace else?
    Posts
    282

    Default Re: Plating Stainless Steel

    Hey, Sean.. How is it going?
    I did give thought to trying some SS Test Pieces, but was also not sure is SS would,
    "somehow" upset the zinc plating bath (I thought I heard that it would "react".. but that
    may just be "old age and confusion" ;-} ).. but you are right about the Dangler.. Never
    really considered that, before (duh...)
    Charles

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

Similar Threads

  1. Stainless Steel Wire General Plating
    By XK120DHC in forum Electroplating Questions
    Replies: 4
    Last Post: 11-14-2009, 12:41 AM
  2. Plating stainless steel watchcase with white gold
    By fredj in forum Electroplating Questions
    Replies: 1
    Last Post: 06-03-2007, 04:58 AM
  3. Tin plating stainless steel
    By jgdpd in forum Electroplating Questions
    Replies: 0
    Last Post: 06-12-2006, 03:46 PM
  4. Stainless steel plating tank
    By Unix3000 in forum Electroplating Questions
    Replies: 3
    Last Post: 02-27-2005, 02:27 PM
  5. Chrome Plating Stainless Steel:
    By rabiddog22 in forum Electroplating Questions
    Replies: 1
    Last Post: 11-23-2002, 05:04 PM

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •