What prep is required?
Remove blueing then polish or vice versa? How do I remove all traces of gunpowder residue and lead? Do I need to plug barrel so it doesn't get nickeled? What sort of plug if yes? Do I need flash copper or can I plat directly over steel? Does flash copper get buffed? If no, would Nickel be dull due to unbuffed copper? |
|
||||
|
Muriatic acid to remove the bluing.
The polish and degrease. Then nickel plate. You CAN plug the barrel, but it shouldn't plate inside because the anodes won't throw inside a barrel. See our tutorial on lines of force on our web site. You can use a plastic plug, or a cork.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Gold Plating and Nickel plating | tzmandevil | Electroplating Questions | 2 | 09-16-2005 09:11 AM |
| How to plate Nickel over old Nickel when steel shows through | ASHENASH | Electroplating Questions | 3 | 04-22-2005 03:03 AM |
| Nickel problems | Eddy | Electroplating Questions | 0 | 04-23-2004 11:31 AM |
| Chrome, Nickel or copy chrome? | dwthomas | Electroplating Questions | 1 | 02-15-2003 01:49 PM |
| Replating Nickel | shorton | Electroplating Questions | 7 | 11-06-2002 11:36 AM |