    Default estimate time for a 4 bl. carb.???

    I recantly glassbeaded my rochester quadrajet and cleaned it out well and dryed it and dipped it into my yellow zinc solution for about 30 sec. and it started to look good but its not dark enough. what would be a good time to set the entire body into it, would 3 to 4 min. be to longDoes it hurt anything to redip after carb. is dry

  2. #2
    MrPontiac is offline Experienced Metal Finisher
    Join Date
    Aug 2006
    Posts
    296

    Default Re: estimate time for a 4 bl. carb.???

    tryed 4 min. and i have a few spots that are not covering, any ideas?? temp was 105

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

Similar Threads

  1. q-jet carb. still trying to plate it! Help
    By MrPontiac in forum Electroplating Questions
    Replies: 6
    Last Post: 08-29-2010, 04:14 PM
  2. anodizing and/or powder coating estimate request
    By baldysm in forum Services Offered/Wanted
    Replies: 0
    Last Post: 06-16-2009, 06:49 PM
  3. also need help on my first estimate!!
    By LNZcustoms in forum Powder Coating Questions
    Replies: 3
    Last Post: 12-19-2006, 05:15 PM
  4. Need help with first real job estimate
    By UnorthodoxCreations in forum Powder Coating Questions
    Replies: 4
    Last Post: 12-19-2006, 02:52 AM
  5. Carb Polishing Help
    By EricWil in forum Metal Polishing Questions
    Replies: 4
    Last Post: 04-16-2006, 07:10 PM

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •