    Default Removing nickel plating from pistol

    Hi, I'am new to this site and I have a Nickel plated pistol that I would like to remove the nickel plating from and then get it Blued.
    What steps do I have to take to strip the nickel off? There is not a plater in this area
    and I would like to do it myself.
    any advice would be helpful-thanks

  2. #2
    lcaswell's Avatar
    lcaswell is offline Caswell Inc President
    Join Date
    Jan 2001
    Location
    Lyons NY USA
    Posts
    643

    Default Re: Removing nickel plating from pistol

    Use B9 stripper. No power needed. No etching of the base metal.

    Caswell Inc. - MetalX Nickel Strippers
    --
    Lance Caswell
    Caswell Inc
    http://www.caswellplating.com
    Need Support? Visit our online support section at http://support.caswellplating.com

    Please support the moderators on our site by leaving reputation for their helpful posts. Read more here.

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

Similar Threads

  1. Nickel plating a pistol
    By Olle in forum Electroplating Questions
    Replies: 24
    Last Post: 09-04-2009, 03:25 PM
  2. removing nickel plating from brass?
    By thomaconda in forum Other Metal Finishing Questions
    Replies: 4
    Last Post: 11-30-2008, 10:35 PM
  3. Removing Nickel Plating
    By drdarvocet in forum Electroplating Questions
    Replies: 8
    Last Post: 11-28-2008, 01:22 PM
  4. removing nickel
    By UFpball7 in forum Electroplating Questions
    Replies: 2
    Last Post: 07-26-2006, 11:11 PM
  5. Brushed Nickel (elect/non-elect) on a Pistol
    By tha3rdman in forum Electroplating Questions
    Replies: 2
    Last Post: 02-10-2003, 02:22 PM

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •