Sorry if this has been covered before but I'm new here. Found this site referenced on Jouster.com. I've got some parade bayonets that I can't seem to sel. Apparently no one wants nickle plated bayonets. What would be the best way to strip the nickle off these so I can parkerize them. Thanks for any and all input.
Phil |
|
||||
|
By using an acid pickle made from diluted battery acid and a stainless steel or lead sheet, you can reverse plate the nickel. This technique is described in detail in our plating manual.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Nickle "Plug-N-Plate" question HELP!! | pyro1711 | Electroplating Questions | 1 | 08-03-2004 10:29 PM |
| Black military finish stripping then nickel plating. | cappi | Electroplating Questions | 0 | 05-06-2004 02:58 PM |
| Stripping anodizing will increase dimensions? | 00_buckshot | Anodizing Questions | 4 | 12-13-2003 07:04 PM |
| stripping smut | johnlindahl | Electroplating Questions | 1 | 11-01-2002 09:57 AM |
| replating nickle on saxophone | JohnF | Electroplating Questions | 4 | 09-15-2002 06:43 PM |