Default Silvaspray on a primered surface

I posted a question awhile back but never got an answer to a problem I had in using Silvaspray. I primered a fiberglass fuel door on a car and then applied the Silvaspray as instructed. After letting it cure for three or four hours, I placed it in the copper bath. When I pulled it out, the copper had plated to the Silvaspray surface but the Silvaspray itself lifted from the primered surface. can you not use Silvaspray over a standard primered surface??
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Something for you die hard polishers out there to chew on thesound Metal Polishing Questions 15 12-03-2007 12:16 PM
Sand blasting media to use for surface prep tavo1765 Powder Coating Questions 13 03-18-2005 11:58 PM
Anodizing without knowing surface area? sbpoole Anodizing Questions 3 01-06-2005 07:09 PM
pimpling surface, please help chrisk Metal Polishing Questions 3 05-22-2004 12:13 AM
SILVASPRAY.....PROBLEM WITH BLISTERING! mdarr Electroplating Questions 2 03-28-2004 09:42 PM


All times are GMT -4. The time now is 10:11 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.