If I use a metal polish with silicone protectants as the last polishing stage prior to Plug N Plate Copy Chroming will it have any effect on the plating process and if so, would cleaning the polished part with laquer thinner be the appropriate last step before plating?
__________________
Scott |
|
||||
|
Yes, it would probably prevent the plate from adhering to the part.
Lacquer thinner/degreaser should remove the layer. You should always degrease before plating to ensure that there are no traces of oil, especially things like fingerprints.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Something for you die hard polishers out there to chew on | thesound | Metal Polishing Questions | 15 | 12-03-2007 01:16 PM |
| Metal Polishing Questions for Nickel Plating | pelletman | Metal Polishing Questions | 3 | 07-31-2004 03:09 AM |
| plug and plating steel rings? | notjustone | Electroplating Questions | 0 | 12-05-2003 05:11 AM |
| Polishing, Chrome Plating and Powder Coating | REVS | Services Offered/Wanted | 0 | 04-19-2003 06:35 PM |