Old 11-13-2003, 05:38 AM
Newbie
 
Join Date: Sep 2003
Posts: 2
mikecurry
Default Plating Through Electro-etch Stencil

Is it possible to use my plug-n-plate kit with my stencil that I currently use with my electro-etch equipment? I'd like to put my logo on a knife blade that I plan to have hot blued. Thought gold or nickel would look nice. Should I plate before or after bluing?

Thanks,
Mike
Reply With Quote
  #2 (permalink)  
Old 11-16-2003, 06:15 AM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,360
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

Seeing as you have both components already, then it looks like you can answer this yourself quite easily.

I can't see any reason whey it won't work, we it's never been tried here.

Please let us know how it works out.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
  #3 (permalink)  
Old 11-17-2003, 08:27 AM
Newbie
 
Join Date: Sep 2003
Posts: 2
mikecurry
Default

I'll do some experimenting and get back to you. I really think that on blued steel, a gold-plate logo would look sharp. My fear is that the plating may "creep" under the stencil and get fuzzy. Only one way to find out...

--Mike Curry
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Gold Plating and Nickel plating tzmandevil Electroplating Questions 2 09-16-2005 09:11 AM
Nickel bath inexplicably quits plating jackf Electroplating Questions 5 01-25-2005 09:55 PM
etching and plating Zippo lighters tbloss001 Electroplating Questions 1 06-26-2003 08:45 PM
plating and size power? chromo Electroplating Questions 7 01-18-2003 02:52 AM
Electroless Krome plating Q's chcarver Electroplating Questions 1 10-10-2002 10:00 PM


All times are GMT -4. The time now is 06:42 AM.


Powered by vBulletin® Version 3.7.0
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.