hi anyone,
im wish to give clients the option of rose gold for their taps along with the usual gold platitun but im finding it had to be able to find any.I understand that the self life on the rose gold isnt very long so only want to buy in smaller quantities.I have read somewhere that if i add coppper strike to the 24kt gold it will produce a rose coloure gold is this correct and is it just as simple as adding half and half copper and gold ?
thanks in advance