I'm using a silver anode to increase the life of the plating solution. Would it work better with a stainless steel anode? hp |
|
||||
|
Sounds like too much power. It will work best with a silver anode, like you had.
For further technical support related questions, we need you to use our PRS system so that we can properly track your problem. The PRS system is located at http://www.caswellplating.com/support.htm Thanks
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| copper over silver | Kurt | Electroplating Questions | 3 | 07-18-2006 01:27 PM |
| I did a dumb thing - now how do I remove copper plating? | Mark3316 | Other Metal Finishing Questions | 0 | 05-19-2005 03:57 PM |
| Differet copper plating questions, plus copy chrome/ nickel? | krsimulis | Electroplating Questions | 1 | 07-26-2004 01:25 AM |
| Silver plating on top of a computer processor | jungle | Electroplating Questions | 5 | 05-13-2004 10:22 PM |
| Silver on copper | hparent | Electroplating Questions | 2 | 03-23-2002 10:40 AM |