Default Re-chroming, Black Chromed Motorcycle Exhaust System

Back in 1983, Honda introduced the CB1100F. An in-line, four cylinder motorcycle that came from the factory with a black chromed exhaust system. Many of these machines still exist today, and many of the owners prefer keeping their machines original. The exhaust system is no longer available from Honda and most of the original pipes have become pitted over time. I am looking for a source of refinishing these OEM exhaust systems for my customers.

Can anyone point me in the right direction?

Thanks,
Michael Rush, Owner
For Hondas Only
Chesterfield, VA
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #2 (permalink)  
Old 12-26-2003, 05:57 AM
Moderator
 
Join Date: Feb 2003
Location: southeast
Posts: 199
bhhodges is on a distinguished road
Default

michael,

caswell sells a black chrome plating kit on the web site . is this what your looking for or someone already set up to do it for you??


bill
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
Closed Thread

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


Similar Threads
Thread Thread Starter Forum Replies Last Post
Painting over chromed plastic &chromed exhaust pipes gkohler Other Metal Finishing Questions 4 07-28-2005 03:07 PM
titanium motorcycle exhaust muffler? mtnbiker Powder Coating Questions 3 04-26-2005 10:01 AM
Need some things Nickel then Black chromed Paintballislife Services Offered/Wanted 0 03-10-2004 03:45 PM
Chromed Plastic to Black Chrome Ultrasparq Electroplating Questions 1 02-18-2004 12:16 AM
Black Chroming in NC? ozziepartsguy2003 Services Offered/Wanted 3 12-18-2003 08:07 PM


All times are GMT -4. The time now is 11:11 AM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2009, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.3.0
Copyright © Caswell Inc.