the best way would be to buy some of caswells gold tank plating solution. i use the fastgold brush plating soultion myself. tank plating is a lot less lobor intensive than any type of brush plating and they both have their pluses and minuses.
what type items are you looking to gold plate?? bill |
|
|||
|
Hello.
I'm an experienced rosary artisan, but novice plater. I wanted to get that same "vermeil" look that I order my parts in, and purchased the plug n plate gold kit. For what I understood, all I had to do was clean it very well, and then plate away. That isn't the case. I cleaned it with sterling silver cleaner, removing all oxidized matter on it, then washed with with warm water and dried it. I followed the instructions that came with the plate system completely, and the gold has a parts with a greenish copper-patina look to it. Reading my Rio Grande catalog, it said you should always nickel plate sterling silver before plating with any type of gold to stop copper color migration, which sterling contains copper. Does this mean I need to purchase the nickel plating kit as well, or what is the deal? Also, the gold is too orangy for my other items, and I was wondering if caswell carries a 14k or 18k gold solution for the plug n plate, or if it's possible to use other brand solutions with the kit I purchased. Obviously, I'm very new, but I'm trying to do my homework. Any detailed instructions on this matter would be greatly appreciated, or feel free to email me directly at info@novenarosary.com . Please no spammers, though. Thanks. |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Gold Plating and Nickel plating | tzmandevil | Electroplating Questions | 2 | 09-16-2005 10:11 AM |
| Silver & Gold Plating Canada | Toocon | Services Offered/Wanted | 0 | 08-26-2004 03:08 PM |
| Plug n Plate Gold over Sterling | novenarosary | Electroplating Questions | 0 | 03-12-2004 11:00 PM |
| Silver plating is looking more like Gold? | guschennells | Electroplating Questions | 1 | 05-11-2003 01:52 PM |
| Silver polish on 24k gold plate?? | chromo | Electroplating Questions | 3 | 04-07-2003 06:14 AM |