I HAVE STRIPPED WASHED, ACTIVATED BUT STLL HAVE SPOTTING...PLEASE READ MY LAST POST...I HAVE GOT TO FIND A SOLUTION FOR THIS...IF THERE IS NOT ONE I HAVE JUST RUINED A VERY EXPENSIVE MOTORCYCLE....AND ITS ALL I HAVE...THANKS
|
|
|||
|
Well:
First off you have not caused irriplacable damage. I doubt if there is any damage at all. You may have to do some stripping and replating though. I would call or mail Caswell about the problem. Its hard to say whats going on without seeing or talking to the person. Your solution may be low in gold. If it came on gradually then thats what I would bet on. That is if you didnt change any of the proceedure. 48Buick |
|
|||
|
THANKS 44 , AT LEAST IVE NOT RUINED ANYTHING...I KEEP CLEANING, STRIPPING BUFFING AND STILL HAVE SPOTS....NO MATTER WHAT I DO...GOLD IS GOOD QUALITY FROM GOLD TOUCH, IN A GEL FORM...I HAVE STRIPPED SO MANY TIMES THERE CAN'T POSSIBLY BE ANY THING LEFT
|
|
|||
|
Quote:
|
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Spots on Aluminum | scocklin | Anodizing Questions | 9 | 06-29-2005 09:51 AM |
| Water spots on "new" aluminum | cwmcobra | Metal Polishing Questions | 5 | 01-19-2004 11:04 PM |
| water spots | shine | Metal Polishing Questions | 2 | 10-16-2003 02:32 PM |
| Removing spots in chrome | dirttracker | Metal Polishing Questions | 3 | 06-21-2003 06:52 AM |