Default Yellow Chromate on Galvanized?

Will yellow chromate coat galvanized metal? Is there some chemical reaction that allows plated zinc to accept the yellow chromate vs a non-plated zinc coating such as cold galvanizing or some of the zinc spray coatings.

Thanks,
__________________
Rickc
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Copy Cad - Yellow Chromate does not stay on charlton Electroplating Questions 1 07-31-2005 11:52 AM
Chromate conversions for CopyCad/Zinc seanc Caswell Please Sell This... 0 03-09-2005 10:44 AM
Copy Cad kit - blackener and yellow cad durability problems Broke Electroplating Questions 11 01-09-2005 10:19 AM
Galvanized, or not Galvanized ? getastro Powder Coating Questions 0 08-08-2003 07:48 PM
Yellow Chromate & Copy Cad aermakov@rogers.com Electroplating Questions 3 03-03-2003 06:28 PM


All times are GMT -4. The time now is 06:33 PM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.