I use silver for brush plating all the time.
I've used both cyanide and alkalie based and I'm just as happy with the non-cyanide solution that Caswell sells as I was with the cyanide stuff. One thing I've noticed (and I'm putting the caveate out there that it may only be "me" who this happens to) is that silver can be very finicky about it's amps. I'll plate fine one day and then use the same setup the next day and find I'm burning the plate. Turns out my rec "drifted" a milliwatt or two and it was enough for the silver plate to burn. (when I say "burn", I mean instead of the plate going on nice and shiny, mirroring the finish, it went on dark and "smudgy". This isn't as terrible as it sounds, as it only takes a little hand polishing to turn the silver shiny again.) To tell you the truth, I've had more problems plating with Nickel than I've every had with Silver. |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Silver plating on top of a computer processor | jungle | Electroplating Questions | 5 | 05-13-2004 10:22 PM |
| Silver plating and rapid tarnish | rustydog | Electroplating Questions | 0 | 04-15-2003 03:43 AM |
| High quality silver plating needed. | clovenguth | Services Offered/Wanted | 0 | 04-02-2003 02:58 PM |
| silver plating | guschennells | Electroplating Questions | 1 | 10-24-2002 01:27 AM |
| Silver Plating on Copper | hparent | Electroplating Questions | 1 | 04-03-2002 06:16 PM |