I went to a shop to have a small auto part that already is anodized blue to be plated with chrome. I was quote around 100 dollars, this seems a bit high to me. They told me they would need to strip the anodizing than polish than plate. Can i do this myself using caswell products but alot cheaper? Would i even need to strip it or could i possibly use copy chrome? Any help would be great. Thanks.