+ Reply to Thread
Results 1 to 2 of 2

Thread: removing copy chrome from aluminum

  1. removing copy chrome from aluminum

    just plated a paintball gun with copy chrome.one side turned out quite well the other side was less than perfect. is there a special proceedure for stripping chrome from aluminum?how do i go about doing this?thanks in advance.
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  2. copy chrome removal

    an up date on my progress. have tried deplating using chrome/ano stripper. had to leave in tank for about 30 min to see any result what so ever.the big problem i am having is that the stripper is removing some spots(on the gun body) faster than others leaving bare spots and alot of pitting. some of the corners on this peice are starting to round-off slightly .need help to remove the rest of this partial plating.help please!
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

+ Reply to Thread

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

     

Similar Threads

  1. copy chrome vs triple chrome plating
    By splbnd27 in forum Electroplating Questions
    Replies: 18
    Last Post: 06-21-2006, 07:35 AM
  2. copy chrome and aluminum problems
    By jtagger19 in forum Electroplating Questions
    Replies: 1
    Last Post: 08-14-2004, 06:15 AM
  3. Copy Chrome Start-up
    By Elitefisherman in forum Electroplating Questions
    Replies: 10
    Last Post: 04-18-2004, 04:24 AM
  4. Removing blistered chrome from aluminum wheels?
    By ozziepartsguy2003 in forum Electroplating Questions
    Replies: 0
    Last Post: 12-14-2003, 06:26 PM
  5. Removing the chrome surface from aluminum based auto trim
    By jbashaw in forum Metal Polishing Questions
    Replies: 6
    Last Post: 10-01-2003, 10:20 PM

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts

Search Engine Friendly URLs by vBSEO 3.5.0 RC1 PL1