Default Gold plating instrument mouthpieces

I am interested in gold plating my silver plated trombone mouthpieces. Is that a possibility? What steps do I need to take, and what gold-plating kits would someone recommend?
Reply With Quote
  #2 (permalink)  
Old 03-20-2004, 09:28 PM
Moderator
 
Join Date: Feb 2003
Location: southeast
Posts: 199
bhhodges is on a distinguished road
Default

its very possible, how many mouth pieces are you thinking of gold plating??


bill
Reply With Quote
  #3 (permalink)  
Old 03-21-2004, 12:23 AM
Newbie
 
Join Date: Mar 2004
Posts: 2
etgreece
Default Mouthpieces

Probably 3 or 4 at the most. Again, my main concerns are having a durable, shiny, consistent finish to hold up to the constant use I put them through. Will it be difficult to get a professional looking finished product?
Reply With Quote
  #4 (permalink)  
Old 01-29-2005, 12:37 AM
Newbie
 
Join Date: Jan 2005
Posts: 1
kowalchuk
Default

You can use the Gold Plug 'n' Plate solution and set it up as a small plating tank. I do screw-rims in gold this way. I do whole MPs using two silver kits (4oz).

John Kowalchuk
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Question on gold plating oldtoys1961 Electroplating Questions 4 05-07-2008 11:41 PM
Gold Plating and Nickel plating tzmandevil Electroplating Questions 2 09-16-2005 10:11 AM
Gold Plating Musical Instrument Parts jedgrhoovr Electroplating Questions 0 04-04-2005 12:48 AM
last step: finishing with wax on gold plating. Which one? didierphmartin Metal Polishing Questions 1 10-29-2004 03:11 AM
gold plating on brass jomida Electroplating Questions 5 02-23-2003 11:34 AM


All times are GMT -4. The time now is 01:39 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.