Default Copy chrome Questions.

How long do the Crystals last (Solution) before needing replaced?
When is Brightener needed?

Thanks in advance
Reply With Quote
  #2 (permalink)  
Old 04-01-2004, 02:51 AM
Newbie
 
Join Date: Mar 2004
Posts: 6
merse1
Default

I did my first item in the Copy Chrome tonight.

A kickstand froma GSXR1000 Sportbike.

IT LOOKS AWSOME!!! I can really tell a difference from Real Chrome.

It is a great product and I can't wait to do more.

Thanks
Reply With Quote
  #3 (permalink)  
Old 04-17-2004, 12:01 AM
Amateur Metal Finisher
 
Join Date: Jul 2002
Location: Florida
Posts: 69
gsw3 is on a distinguished road
Default How long do the solutions last

I have had my Copy Chrome solution for almost (2) years.
Some of my nickel solution is (5) years old.

Don't get any zinc metal in it, filter it using the large coffee filters about once a month (depends on usage) and top off the evaporation with only distilled water.
Be sure and use the "Bandage" over the nickel anodes.
Otherwise the black deposits will get in your solution and may pit your parts.

Always pull out the anodes, wash them off and wash the bandage after every plating session.

The solution should out last you if you do all of the above.

George W.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
copy chrome vs triple chrome plating splbnd27 Electroplating Questions 18 06-21-2006 08:35 AM
Differet copper plating questions, plus copy chrome/ nickel? krsimulis Electroplating Questions 1 07-26-2004 01:25 AM
Copy Chrome Start-up Elitefisherman Electroplating Questions 10 04-18-2004 05:24 AM
Copy Chrome Questions junodale Electroplating Questions 13 03-17-2004 12:15 PM
Copy Chrome Immersion system questions. Great_Scott Electroplating Questions 3 03-20-2002 06:52 PM


All times are GMT -4. The time now is 01:47 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.