Experienced Metal Finisher
 
Join Date: Apr 2004
Posts: 466
jtagger19 is on a distinguished road
Default electroless nickel over plastic

hey guys I have a Q
can electroless nickel plating be done over plastic ?
I've been reading on this forum and to electroplate over plastic you have to use silvachrome spray to make the part conductive
but since I will be ussing an electroless kit
will it work without the silvachrome?
Reply With Quote
  #2 (permalink)  
Old 04-14-2004, 08:48 PM
customandsound
Guest
 
Posts: n/a
Default

try it out and start a post about the way you did it ....
Reply With Quote
  #3 (permalink)  
Old 04-14-2004, 10:22 PM
Moderator
 
Join Date: Feb 2003
Location: southeast
Posts: 199
bhhodges is on a distinguished road
Default

as long as the part is conductive i dont see any reason it wouldnt work. post your steps for everyone to see.


bill
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
"high phosphorus" electroless nickel? jkellymcc Electroplating Questions 0 08-26-2003 06:35 PM
electroless nickel vs regular nickel Rocky Electroplating Questions 1 07-24-2003 03:12 PM
Pot Metal Electroless Nickel - Suitability as finish tgoode Plating Pot Metal 6 06-17-2003 08:01 PM
Electroless Nickel over Chrome gglines Electroplating Questions 1 05-13-2002 12:09 AM
tank for electroless nickel jpb531 Electroplating Questions 1 04-03-2002 06:18 PM


All times are GMT -4. The time now is 01:38 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.