Default Electroless Krome VS Copy Chrome plating?

Whats the diff? i read up on both of them but still don't quite get what the diff is. I like the fact that copy chrome doesn't use any harsh chemicals or produces fumes and what not, so what about the electroless krome though?

which is better for small automotive parts? Which will come out nicer and more like real triple plate? Which will be faster? Thanks

rob.
Reply With Quote
  #2 (permalink)  
Old 04-28-2004, 04:44 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,361
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

They both give the same result and have the same properties. Electroless plating is ideally suited for plating inside tubes and deep recessed areas.

Most applications call for regular electroplating, not electroless.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
  #3 (permalink)  
Old 04-28-2004, 06:04 PM
Newbie
 
Join Date: Feb 2004
Posts: 12
qwik3r
Default

I see that the Electroless Krome mini package is alot cheaper than the Copy Chrome kit, i figure i would not be able to get alot done with it but does it come with everything to clean the parts? I primarily want to just do nuts/bolts and also a few small engine parts like brackets and what not. Will i run out of whatever it comes with quickly? Thanks

rob.
Reply With Quote
  #4 (permalink)  
Old 04-28-2004, 11:39 PM
Newbie
 
Join Date: Feb 2004
Posts: 12
qwik3r
Default

So what exactly is involved with this electroless krome kit? I don't have access to alot of tools and chroming car parts for my car is more of a hobby for shows. Do you need to heat the solution up with an oven, or a hot plate or what? Can i throw a bunch of stuff in at a time like nuts and bolts and brackets/hinges? Thanks
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
copy chrome vs triple chrome plating splbnd27 Electroplating Questions 18 06-21-2006 07:35 AM
Differet copper plating questions, plus copy chrome/ nickel? krsimulis Electroplating Questions 1 07-26-2004 12:25 AM
Copy Chrome Start-up Elitefisherman Electroplating Questions 10 04-18-2004 04:24 AM
Price of Copy Chrome vs. electroless Krome plating dwthomas Electroplating Questions 1 05-14-2003 10:01 AM
Electroless Krome plating Q's chcarver Electroplating Questions 1 10-10-2002 10:00 PM


All times are GMT -4. The time now is 12:53 AM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.