I want to start chrome plating. I have never done it, and don't know a whole lot about it. Could some one please give me some tips on the best way to get started. What kit would be best / easiest? How large of parts can I do with each kit? Any help is appreciated.
Kris |
|
|||
|
first decide what is the largest sized part you think you will plate. the type of base metal is a very important factor in what type set up your going to need as well. for an example --- if i was only going to nickel plate brass base items then all i would need is nickel and then chrome. also try and invest into a variable power supply that is adjustable in both amperage and voltage.
id recommend trying to get 2 out of the three steps down before trying to do a full "triple" plate with chrome. or just try nickel plating some brass which is about the easiest metal to plate onto. bill |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Getting Started... | THOR4LIFE | Anodizing Questions | 3 | 07-17-2005 06:15 PM |
| Newbie here getting started today! Hello everybody! | boogerboy | Metal Polishing Questions | 2 | 02-04-2005 11:40 PM |
| Powder Coating Started Kit | PhilipK | Powder Coating Questions | 1 | 12-18-2004 08:28 PM |
| wanting to get started in powdercoating | BRANDONPEAKE | Powder Coating Questions | 13 | 01-10-2004 10:38 AM |
| Getting started | pballclerk | Electroplating Questions | 1 | 05-05-2003 09:29 PM |