hellos
Default Question on heat transfer on final part.

Hello, I am plating an intake manifold that sees temp of up to 250 deg. for a cust. He wanted to know if the plating would hold the heat into the part and cause higher temps. It is an aluminum manifold which will be copper, zinc,chromium plated. I don't think it will matter one bit, but he is worried. Thanks in advance for any help.
-John
Reply With Quote
  #2 (permalink)  
Old 06-16-2004, 08:36 AM
Newbie
 
Join Date: Jun 2004
Posts: 2
hellos
Default

Bump, Anyone have any ideas on this. I tried the search function but cound not come up with anything.
Reply With Quote
  #3 (permalink)  
Old 06-26-2004, 03:51 PM
Moderator
 
Join Date: Feb 2003
Location: southeast
Posts: 199
bhhodges is on a distinguished road
Default

here is a piece i just baked for 1/2 hour at 500 degrees .





bill
Reply With Quote
  #4 (permalink)  
Old 06-26-2004, 03:54 PM
Moderator
 
Join Date: Feb 2003
Location: southeast
Posts: 199
bhhodges is on a distinguished road
Default

i dont think the thin plating with hold in more heat to create more heat



bill
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Aluninum heat transfer rate. levi Powder Coating Questions 6 10-14-2006 11:05 AM
?1) blast cabinet replacement part ?2) exhaust heat shields upncoming Powder Coating Questions 4 03-21-2005 12:33 PM
A few question to help a beginner Cyberave68 Anodizing Questions 6 06-08-2004 08:53 PM
Peak voltage question mudwhump Anodizing Questions 6 01-14-2004 10:53 PM


All times are GMT -4. The time now is 02:13 PM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.