I am trying to figure out how to use the triple chrome plating system to plate aluminum, so I can get a kit. Do I have to use the flash copper with the zincated aluminum, or can I just use the regular copper plating system. If I do have to use the flash copper, can I then go to the nickel right after that.
Is there another way people plate aluminum. I bought an aluminum piece that someone chromed, and it wasn't plated all around, and there was no trace of the pre zincate. I think I remember reading something about people using cyanide or something like that. Just curious how that was possible. thanks, Kenny |
|
|||
|
you do not have to use any copper plating on it as long as its in good shape, you must zincate then nickel plate though.
the pick a kit helper on the home page will answer this same question and others similar to it as well. bill |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Something for you die hard polishers out there to chew on | thesound | Metal Polishing Questions | 15 | 12-03-2007 12:16 PM |
| Flash Copper Problem | gwjohnso | Plating Pot Metal | 12 | 02-27-2007 11:41 PM |
| Keep getting blisters in flash copper plating...HELP | gtabadboy | Electroplating Questions | 7 | 11-17-2005 08:19 PM |
| Newbie ? on copychome and flash copper? | KevinW | Plating Pot Metal | 3 | 11-08-2002 12:49 PM |